SlideTinA
TiNa-A

Properties of TiNa-A(TiAlN) coating.
- Increasing tool life.
- High heat resistance.
- High scratch resistance.
Maximum operate temperature around 900 degree Celsius.
Coating thickness 3 - 4 micron.
Visual color dark purple.
Suitable for high speed cutting tools for hardness material, etc.

.
.
.
.

previous arrowprevious arrow
next arrownext arrow
Shadow

What is PVD?

 Physical Vapor Deposition (PVD) is widely used technique for the superior features than general tools such as increase tool life, Lubricataion, Wear resistance, etc. of tools. PVD has been used a lot at the industrial scale especially automotive part and mold makerฺ

Basic on coating.

 A coating is a hard thin film (micrometer unit), adhesion layer of chemical compound that us applied to a workpiece.

 - Increased tool life / wear resistance.
   With high hardness and low coefficient of friction will help the surface material to bear less load. Which will also reduce the wear of the material.
 - Increase production efficiency
   The coating can increase the cutting speed, reduce maintenance time.
 - reduce cost
   Reduce wear and increase service life Will help save on buying or creating new tools

The following table show you a comparison of the different technicial parameter of the six coatings.

TiNa-A GolA GiaN TiNa-C TiNa-AT CroM
Composition TiAlN/TiN TiN AlCrN TiCN TiAlN/TiN CrN
Hardness (HV) 3700 2700 3700 3000 4000 2250
Standard Thickness (μm) 2.0-4.0 2.5-4.0 3.0-5.0 3.0-6.0 6.0-16.0 6.0-18.0
Maximum Operate Temp. (℃) 900 600 1,037 400 900 600
Visual Color

Additional coating information

Avatar








TiNa-A

Titanium Aluminium Nitride (TiAlN)

Avatar








GolA

Titanium Nitride (TiN)

Avatar








GiaN

Aluminium Chromium Nitride (AlCrN)


Avatar








TiNa-C

Titanium Carbo Nitride (TiCN)

Avatar








TiNa-AT

Titanium Aluminium Nitride (TiAlN Extra Thin)

Avatar








CroM

Chromium Nitride (CrN)